镍合金机械加工辊环锻件产品对标技术方案

发布日期:2024年08月01日


编制单位:贵州航宇科技发展股份有限公司

参编单位:

方案编号:CS4437-20240717

标准号:AMS5707

标准名称:Nickel Alloy, Corrosion- and Heat-Resistant.Bars, Forgings, Rings, and Forging Stock 57Ni-19.5Cr-13.5Co-4.3Mo-3.0Ti-1.4A1-0.05Zr-0.006B Consumable Electrode Remelted or Vacuum induction Melted 1825 to 1900 °F(996 to 1038 °C)...

序号 关键指标名称 指标值 试验/评价方法标准
1 Combination Stress Rupture Test Temperature (F) 1350 ASTM E292
2 Room Temperature Tensile Elongation in 4D (%) ≥15 ASTM E8/E8M
3 Room Temperature Tensile Reduction of Area (%) ≥18 ASTM E8/E8M
4 Room Temperature Tensile 0.2% Offset Yield Strength (ksi) ≥110 ASTM E8/E8M
5 Room Temperature Tensile Ultimate Tensile Strength (ksi) ≥160 ASTM E8/E8M
6 Smooth Stress Rupture Test Temperature (F) 1500 ASTM E 139
7 "Combination Stress Rupture Stress Level (ksi)" ≥75 ASTM E292
8 Smooth Stress Rupture Final Time (hrs) ≥23 ASTM E 139
9 Grain Size Determination ASTM 3.0 or finer ASTM E112
10 Smooth Stress Rupture Elongation in 4D (%) ≥5 ASTM E 139
11 Combination Stress Rupture Final Time (hrs) ≥23 ASTM E292
12 Combination Stress Rupture Elongation in 4D (%) ≥8 ASTM E292
13 "Smooth Stress Rupture Stress Level (ksi)" ≥40 ASTM E 139
14 Hardness Testing- Brinell(HBW 10/3000kg) 321~437 ASTM E10